Eastman Drystar 0601 Copolyester, Film
Subcategory: Polyester, TP; Thermoplastic; Polymer
Material Notes: Eastman is pleased to announce the launch of DRYSTAR* copolyesters. This new product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellent balance of properties such as superior aesthetics, impact strength, and chemical resistance. These properties can be optimally realized when the resins are properly dehydrated in accordance to recommended drying conditions and equipment.Recognizing this value, Eastman conceived DRYSTAR copolyesters to allow converters with limited access to desiccant dryers to achieve these optimizations. In addition, some converters with desiccant dryers may still find DRYSTAR copolyesters value-adding to attain production flexibility and cost saving by removing the drying process prior to injection molding, profile extruding, or extrusion blow molding copolyesters. The initial launch comprises of the commercialization of four grades of DRYSTAR copolyesters and Eastman has on-going program to extend this strategic product-line in the future. *DRYSTAR is only available in the Asia Pacific Region. Applications/Uses Injection molding
| Available Properties |
- Specific Gravity
- Water Vapor Transmission
- Oxygen Transmission
- Carbon Dioxide Transmission
- Viscosity Measurement
- Thickness
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Film Elongation at Yield, MD
- Film Elongation at Yield, TD
- Tensile Modulus
- Tear Strength
- Tear Strength, Total
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Haze
- Gloss
- Transmission, Visible
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|