Eastman DuraStar DS1000 Polymer, Natural
Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT)
Material Notes: Durastar DS1000 polymer has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS1000 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily, fills intricate molds, and is well suited for thick-wall applications. Under existing United States Food and Drug Administration (FDA) regulations, Durastar DS1000 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.Applications/Uses Floor careHousewaresToys/Sporting goodsFurniture/Furniture trimPoint of purchase displaysWriting instrumentsKey Attributes Good chemical resistanceExcellent flowOutstanding impact resistanceExcellent clarityFast drying timesQuick cycle times
| Available Properties |
- Density
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Notched, Low Temp (ISO)
- Impact Test
- Izod Impact, Notched @ -40°C
- Izod Impact, Unnotched @ -40°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Haze
- Transmission, Visible
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|