Eastman DuraStar DS2110UVI Polymer, Natural
Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT)
Material Notes: Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent light. It has excellent appearance and is nearly water-clear. Its other most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2110UVI has very good toughness as shown by Izod impact resistance. Easy to process, it flows readily, fills intricate molds, and contains a mold release. This product is certified to ANSI/NSF Standard 51.Applications/Uses AppliancesFurniture/Furniture trimToys/Sporting goodsHousewaresPoint of purchase displaysKey Attributes Good chemical resistanceExcellent flowOutstanding impact resistanceExcellent clarityFast drying timesQuick cycle times
| Available Properties |
- Density
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Notched, Low Temp (ISO)
- Impact Test
- Izod Impact, Notched @ -40°C
- Izod Impact, Unnotched @ -40°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Haze
- Transmission, Visible
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|