Eastman Eastar 21446 Copolyester
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Eastar Copolyester 21446 is a brilliantly clear polymer with excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.
| Available Properties |
- Density
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Impact Test
- Izod Impact, Notched @ -40°C
- Izod Impact, Unnotched @ -40°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Color, CIE b*
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|