Eastman Eastar EB062 Copolyester
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to commonly used materials, Eastar copolyester EB062 runs on most standard processing equipment. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles.Applications/Uses Beverage packagingBottlesExtrusion blow moldingFood packagingKey Attributes Effective barrier propertiesExcellent ClarityExcellent colorabilityGood stiffnessExcellent chemical resistanceToughnessEasy to extrude, cut, print, and sealHigh gloss appearanceGood impact strength
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Impact Test
- Izod Impact, Notched @ -40°C
- Izod Impact, Unnotched @ -40°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|