Eastman Eastar GN078 Copolyester, Natural
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Eastar Copolyester GN078 builds on the strength of Eastar Copolyester GN077 by offering improved melt strength and toughness. Eastar Copolyester GN078 does not meet FDA compliance but is an excellent product for large tough bottles not requiring this approval. Eastar Copolyester GN078 is an environmentally responsible material that contains no halogens or orthophthlate plasticizers.Applications/Uses Non-FDA EBM applications
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Impact Test
- Izod Impact, Notched @ -40°C
- Izod Impact, Unnotched @ -40°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|