Eastman Eastar MN003 Copolyester
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Eastar Copolyester MN003 has excellent flow characteristics while maintaining superior mechanical properties. It is easy to process and can fill intricate tools. Its most outstanding features are clarity, toughness and chemical resistance.Applications/Uses MedicalMedical Devices
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Impact Test
- Izod Impact, Notched @ -40°C
- Izod Impact, Unnotched @ -40°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Haze
- Transmission, Visible
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|