Eastman Eastobond 19411 Copolyester, Film
Subcategory: Polyester, TP; Thermoplastic; Polymer
Material Notes: Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low softening point, enabling heat-seal bonds to be achieved over a temperature range of 95°C to 205°C.
| Available Properties |
- Density
- Specific Gravity
- Bulk Density
- Melt Density
- Water Vapor Transmission
- Oxygen Transmission
- Carbon Dioxide Transmission
- Viscosity Measurement
- Thickness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Elmendorf Tear Strength, MD
- Specific Heat Capacity
- Thermal Conductivity
- Glass Temperature
- Haze
- Gloss
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|