Eastman Eastobond 19412 Copolyester, Film
Subcategory: Polyester, TP; Thermoplastic; Polymer
Material Notes: Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastobond 19412 may be dried in a desicated drying system at 150 F. It offers excellent organoleptic and gas-barrier properties. Eastobond 19412 has low postextrusion crystallinity and a low softening point, enabling heat-seal bonds to be achieved over a temperature range of 95°C to 205°C.
| Available Properties |
- Density
- Specific Gravity
- Bulk Density
- Melt Density
- Water Vapor Transmission
- Oxygen Transmission
- Carbon Dioxide Transmission
- Viscosity Measurement
- Thickness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Elmendorf Tear Strength, MD
- Specific Heat Capacity
- Thermal Conductivity
- Glass Temperature
- Haze
- Gloss
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|