Hifor LT74119-F Polyethylene Film, Using Energx (SM) Technology Services
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Hifor Polyethylene LT74119-F is a high strength linear polyethylene containing medium slip and high antiblock and it contains processing aid. It is designed for blown film applications and is well suited for consumer and industrial packaging markets which require good impact and tear strength. Films produced using LT74119-F exhibit low imperfections and facilitate product at thinner gauges.Applications/Uses Industrial packagingBlown film
| Available Properties |
- Base Resin Density
- Thickness
- Base Resin Melt Index
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Heat Seal Strength Initiation Temperarture
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|