Eastman Mxsite LC78104-C Polyethylene Film, Using Energx (SM) Technology Services
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: Mxsite LC78104-C polyethylene is recommended for the skin layers of cast stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling force comes without a substantial increase in film unwind force. It is designed for machine wrap and hand wrap applications where good processability, low gel content and substantial cling are needed. It can be used as cling layer in many "one-sided cling" films because it clings very well to many non-cling resins.Applications/Uses Cast filmFilmsStretch film
| Available Properties |
- Base Resin Density
- Thickness
- Base Resin Melt Index
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Haze
- Gloss
- Peel Cling, Aged 2 Weeks, 0%
- Peel Cling, Aged 2 Weeks, 200%
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|