Mxsten CV77523-F Plastomer Film
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Film
Material Notes: Mxsten CV plastomer CV77523-F is a polyethylene plastomer designed for blown film extrusion that contains high slip, high antiblock and high processing aid additives. Films produced with this resin exhibit exceptionally low seal initiation temperature with a broad hot tack window combined with good stiffness. Other features of this resin include extreme strength in cold and refrigerated temperature environments, high resistance to tears, and high MVTR.Applications/Uses Cast filmBlown FilmShrink filmFood packaging
| Available Properties |
- Base Resin Density
- Thickness
- Base Resin Melt Index
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Heat Seal Strength Initiation Temperarture
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|