Eastman Neostar FN005 Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Polyester TPE
Material Notes: Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where toughness and flex-crack resistance are required. Neostar FN005 can be used in injection molding and cast film or tubing extrusion applications or in any application that demands strength, durability, and puncture resistance in harsh environments. This copolyester combines toughness, clarity, and flexibility without the addition of plasticizers. Neostar FN005 is considered environmentally preferred because of its non-halogenated material composition. The target inherent viscosity of this product is 1.05.Applications/Uses AutomotiveFlexible hingesPricing channelsRetail pricing finsDriver and passenger side air bagsPackagingProfilesTubingKey Attributes Environmentally preferred, non-halogenated materialExcellent chemical resistanceExceptional heat resistance and high temperature dimensional stabilityHigh flexibility without plasticizersSolvent bondable
| Available Properties |
- Specific Gravity
- Water Absorption
- Viscosity Measurement
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Tear Strength, Total
- Izod Impact, Notched @ -40°C
- Heat of Fusion
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Crystallization Temperature
- Vicat Softening Point
- Brittleness Temperature
- Glass Temperature
- Clash Berg Stiffness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|