Eastman Provista ST Copolymer
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation material that complements Provista by offering similar features, while providing greater toughness. Provista Copolymer ST is ideal in applications that place greater physical demands on the profile.Applications/Uses Packaging tubesPricing channelsSignage channelsPlastic angle moldingsProfilesStore fixturesKey Attributes Ease of processingExcellent chemical resistanceMeets FDA regulations for food contactSparkling clarity and high glossToughness with flexibility
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Impact Test
- Izod Impact, Notched @ -40°C
- Izod Impact, Unnotched @ -40°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|