Eastman Spectar 14471 Copolyester
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use thinner-gauge sheet than with other common materials, resulting in lower material costs. Yet it can be extruded into sheets as thick as 12 mm (1/2 in.). It extrudes at a low temperature and will not crystallize or develop a crystalline haze. Cleaning solutions will not turn Spectar copolyester white. It is easy to fabricate, allowing greater design freedom. It can be laser cut, routed, welded, drilled, die-punched, bent hot or cold, or joined by screws, rivets, or bolts. It can also be cut on conventional table, band, or radial-arm saws with blades commonly used for plastic. Spectar copolyester can be vacuum-formed at lower temperatures than other plastics without predrying the sheet. Spectar copolyester can be finished easily. Its edges can be polished by using commercial edge-finishing equipment, sanding, solvents, flame-polishing or buffing. It forms clear, strong bonds with commercially available cements and solvents. It accepts screen-printing, painting, and hot-stamping easily. Surface scratches or scuff marks can be removed using a common heat gun.Applications/Uses Furniture/Furniture trimPoint of purchase displaysSignsKey Attributes Good chemical resistanceEasy to print and decorateOdorlessOutstanding toughness allows downgaugingVersatile - easy to fabricateExcellent clarityExcellent thermoforming characteristicsOutstanding impact resistanceResists chipping and cracking
| Available Properties |
- Density
- Specific Gravity
- Water Absorption
- Thickness
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched Low Temp
- Izod Impact, Notched, Low Temp
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Impact Test
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Refractive Index
- Haze
- Gloss
- Yellow Index
- Transmission, Visible
- Color, CIE b*
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|