Eastman TiGlaze ST Copolyester
Subcategory: Polyester, TP; Thermoplastic
Material Notes: TiGLAZE ST Copolyester is copolyester engineered for the Architectural Glazing industry. TiGLAZE ST offers a combination of strength and fabrication performance for glazing applications such as skylights, vaults, shelters and building entries. The material failed to discharge under a Static Decay Rate test ASTM D4470.Applications/Uses Architectural glazingSkylights
| Available Properties |
- Density
- Water Absorption
- Viscosity Measurement
- Thickness
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Izod Impact, Unnotched Low Temp
- Izod Impact, Notched, Low Temp
- Impact Test
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Arc Resistance
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Haze
- Gloss
- Yellow Index
- Transmission, Visible
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|