Eastman Tsunami GS1 Copolyester Film

 

Subcategory: Polyester, TP; Thermoplastic; Polymer

Material Notes:
Tsunami copolyester is an Eastman Specialty Plastic developed for the calendering industry. It can be used on existing calendering lines with no or minimal modification. Tsunami copolyester is used for decorative lamination. This product is only available in Europe and Asia.

Applications/Uses

  • Laminating
  • Available Properties
    • Density
    • Specific Gravity
    • Water Absorption
    • Water Vapor Transmission
    • Oxygen Transmission
    • Viscosity Measurement
    • Thickness
    • Film Tensile Strength at Yield, MD
    • Film Tensile Strength at Yield, TD
    • Film Tensile Strength at Break, MD
    • Film Tensile Strength at Break, TD
    • Film Elongation at Break, MD
    • Film Elongation at Break, TD
    • Film Elongation at Yield, MD
    • Film Elongation at Yield, TD
    • Tensile Modulus
    • Impact Test
    • Elmendorf Tear Strength, MD
    • Elmendorf Tear Strength, TD
    • Volume Resistivity
    • Surface Resistivity per Square
    • Dielectric Constant
    • Dielectric Strength
    • Dissipation Factor
    • Arc Resistance
    • CTE, linear 20°C
    • Specific Heat Capacity
    • Deflection Temperature at 0.46 MPa (66 psi)
    • Deflection Temperature at 1.8 MPa (264 psi)
    • Vicat Softening Point
    • Glass Temperature
    • Oxygen Index
    • Haze
    • Gloss
    • Transmission, Visible
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。