Eastman Tsunami GS1 Copolyester Film
Subcategory: Polyester, TP; Thermoplastic; Polymer
Material Notes: Tsunami copolyester is an Eastman Specialty Plastic developed for the calendering industry. It can be used on existing calendering lines with no or minimal modification. Tsunami copolyester is used for decorative lamination. This product is only available in Europe and Asia.Applications/Uses Laminating
| Available Properties |
- Density
- Specific Gravity
- Water Absorption
- Water Vapor Transmission
- Oxygen Transmission
- Viscosity Measurement
- Thickness
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Film Elongation at Yield, MD
- Film Elongation at Yield, TD
- Tensile Modulus
- Impact Test
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- Specific Heat Capacity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Oxygen Index
- Haze
- Gloss
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|