Eastman Vitiva PC715 PET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damaging wavelengths of light, protecting the contents of the package. In addition, Vitiva PET allows brand owners to achieve uniquely shaped containers with extraordinary clarity thereby showcasing the contents of the package.Applications/Uses CosmeticsHealth and nutrition containersHousehold products containersPharmaceutical containersCustom bottlesHotfilled food and beverage containersPersonal careKey Attributes Chemical compatibility with packaged goodsDrop-in replacement for standard PETExceptional drop impact strengthMeets FDA regulations for food contactUnlimited recyclabilityExcellent clarityExcellent oxygen gas barrierFDA-compliant UV light barrierVirtually unlimited bottle design freedom
| Available Properties |
- Density
- Bulk Density
- Melt Density
- Particle Size
- Viscosity Measurement
- Heat of Fusion
- Specific Heat Capacity
- Melting Point
- UV Transmittance
- Acetaldehyde
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
- Fines, wt%, max
- Pellet Shape
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|