Voridian Aqua WA314 PET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Voridian Aqua PET WA314 is a polyethylene terephthalate resin designed for single-serve bottled water applications. WA314 has an intrinsic viscosity of 0.76 and provides sparkling clarity and fast injection molding cycles.Applications/Uses Water bottlesKey Attributes Fast injection molding cyclesSparkling clarity
| Available Properties |
- Bulk Density
- Melt Density
- Viscosity Measurement
- Melting Point
- Acetaldehyde
- Color, CIE L*
- Fines, wt%, max
|
|
|
|