Voridian PET 5214A
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containers used in the pharmaceutical industry. Voridian PET 5214A has Drug Master File No. 9987 filed with the U.S. FDA and is commercially available in the United States, Canada, Mexico, Europe, Australia, and New Zealand. Applications/Uses Automotive parts containersFood packagingHousehold products containersPharmaceutical containersKey Attributes BrightTransparent
| Available Properties |
- Density
- Bulk Density
- Melt Density
- Particle Size
- Viscosity Measurement
- Heat of Fusion
- Specific Heat Capacity
- Melting Point
- Acetaldehyde
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
- Fines, wt%, max
- Pellet Shape
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|