Voridian PET 9921P Injection Molded
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia, Brazil, Chile, Colombia, Mexico, Paraguay, Peru, Uruguay and Venezuela. Voridian PET 9921P will be used primarily for thick wall applications such as refill bottles for water and carbonated soft drinks.Applications/Uses APET and thick sheetBeverage packagingCustom containersThick wall containersBottlesSealing layer for CPET traysRefillable bottles
| Available Properties |
- Density
- Specific Gravity
- Bulk Density
- Melt Density
- Viscosity Measurement
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched Low Temp
- Izod Impact, Notched, Low Temp (ISO)
- Impact Test
- Izod Impact, Notched @ -40°C
- Izod Impact, Notched
- Heat of Fusion
- Specific Heat Capacity
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Acetaldehyde
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
- Fines, wt%, max
- Pellet Shape
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|