Voridian PET 9921W Injection Molded

 

Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic

Material Notes:
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It is a copolymer PET that has been crystallized. Color concentrates, additives, and denest versions of 9921 are available on request.

Applications/Uses

  • APET sheet
  • Automotive parts containers
  • Food packaging
  • Household products containers
  • Pharmaceutical containers
  • Wine and liquor containers
  • Water bottles
  • Carbonated soft drink bottles
  • Available Properties
    • Density
    • Specific Gravity
    • Bulk Density
    • Melt Density
    • Particle Size
    • Viscosity Measurement
    • Hardness, Rockwell R
    • Tensile Strength at Break
    • Tensile Strength, Yield
    • Elongation at Break
    • Tensile Modulus
    • Flexural Modulus
    • Flexural Yield Strength
    • Izod Impact, Notched (ISO)
    • Izod Impact, Unnotched
    • Izod Impact, Unnotched Low Temp
    • Izod Impact, Notched, Low Temp (ISO)
    • Impact Test
    • Izod Impact, Notched @ -40°C
    • Izod Impact, Notched
    • Heat of Fusion
    • Specific Heat Capacity
    • Melting Point
    • Deflection Temperature at 0.46 MPa (66 psi)
    • Deflection Temperature at 1.8 MPa (264 psi)
    • Acetaldehyde
    • Color, CIE a*
    • Color, CIE b*
    • Color, CIE L*
    • Fines, wt%, max
    • Pellet Shape
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。