Voridian PET CB11E
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and better bottle properties. CB11E is formulated to provide improved efficiencies in preform and bottle production while delivering a robust processing window. Bottles made with this polymer deliver improved barrier with continued excellent performance in creep and environmental stress-crack resistance.Applications/Uses Carbonated soft drink containersBeverage PackagingBottles
| Available Properties |
- Density
- Bulk Density
- Melt Density
- Particle Size
- Viscosity Measurement
- Heat of Fusion
- Specific Heat Capacity
- Melting Point
- Acetaldehyde
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
- Fines, wt%, max
- Pellet Shape
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|