Voridian PET CB12

 

Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic

Material Notes:
Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good overall bottle properties. This polymer is formulated to provide improved efficiencies in preform and bottle production while delivering a robust processing window. Bottles made with CB12 deliver improved barrier with continued excellent performance in creep and environmental stress-crack resistance.
The pellets have a weight of 2.0g/100pellets

Applications/Uses

  • Bottles
  • Carbonated soft drink containers
  • Key Attributes

  • Excellent performance in stress-crack resistance
  • Fast, efficient processing
  • Improved barrier
  • Robust processing window
  • Available Properties
    • Density
    • Bulk Density
    • Melt Density
    • Particle Size
    • Viscosity Measurement
    • Heat of Fusion
    • Specific Heat Capacity
    • Melting Point
    • Acetaldehyde
    • Color, CIE a*
    • Color, CIE b*
    • Color, CIE L*
    • Fines, wt%, max
    • Pellet Shape
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。