Voridian PET CB12
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good overall bottle properties. This polymer is formulated to provide improved efficiencies in preform and bottle production while delivering a robust processing window. Bottles made with CB12 deliver improved barrier with continued excellent performance in creep and environmental stress-crack resistance. The pellets have a weight of 2.0g/100pelletsApplications/Uses BottlesCarbonated soft drink containersKey Attributes Excellent performance in stress-crack resistanceFast, efficient processingImproved barrierRobust processing window
| Available Properties |
- Density
- Bulk Density
- Melt Density
- Particle Size
- Viscosity Measurement
- Heat of Fusion
- Specific Heat Capacity
- Melting Point
- Acetaldehyde
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
- Fines, wt%, max
- Pellet Shape
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|