Voridian PET P76CC
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Voridian PET P76CC is used for dual ovenable containers and release paper.Applications/Uses Dual ovenable containersRelease paper
| Available Properties |
- Density
- Bulk Density
- Melt Density
- Viscosity Measurement
- Melting Point
- Acetaldehyde
- Color, CIE a*
- Color, CIE b*
- Color, CIE L*
- Fines, wt%, max
|
|
|
|