Eastman Chemical Polyethylene 1925F Film
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarity is important. Common applications include bread bags, fresh produce bags, and converter film requiring printability. An additive in this formulation limits the use of 1925F to nonalcoholic foods, and the average thickness of such polymers in the form in which they contact food shall not exceed 0.0050 inch. Users must make their own determination of its safety, lawfulness, and technical suitability in their intended applications.Applications/Uses Bread bagsProduce bags
| Available Properties |
- Base Resin Density
- Water Vapor Transmission
- Oxygen Transmission
- Thickness
- Base Resin Melt Index
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|