Eastman Chemical Polyethylene E6838-913P
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: Polyethylene E6838-913P natural is a specialty formulation suggested for high-speed extrusion coating applications. E6838-913P offers improvements over standard low-density polyethylene in adhesion to foil.Applications/Uses Foil
| Available Properties |
- Density
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|