Eastman DURASTAR Polymer DS1010 Natural PCTA Copolyester
Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT); Polymer
Key Words: Polycyclohexylenedimethylene Terephthalate
Material Notes: Product Description: DURASTAR DS1010 polymer contains a mold release. It has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS1010 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily, fills intricate molds, and is well suited for thick-wall applications. Under existing United States Food and Drug Administration (FDA) regulations, DURASTAR DS1010 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.
Applications: Appliances; Furniture/Furniture trim; Point of purchase displays; Toys/Sporting goods
Technical Data Sheet
Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given. Information provided by Eastman Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Haze
- Transmission, Visible
- Processing Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|