Eastman DURASTAR Polymer DS2010 Natural PCTA Copolyester
Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT); Polymer
Key Words: Polycyclohexylenedimethylene Terephthalate
Material Notes: Product Description: DURASTAR DS2010 polymer contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2010 has very good toughness as shown by Izod impact resistance. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS2010 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Under existing United States Food and Drug Administration (FDA) regulations, DURASTAR DS2010 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.
Applications: Floor care; Furniture/Furniture trim; Housewares; Point of purchase displays; Toys/Sporting goods; Writing instruments
Technical Data Sheet
Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given. Information provided by Eastman Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Haze
- Transmission, Visible
- Processing Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|