Eastman EASTAR Copolyester BR003, Natural PCTA Copolyester
Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT)
Key Words: Polycyclohexylenedimethylene Terephthalate
Material Notes: Product Description: EASTAR BR003 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but BR003 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. BR003 is specifically formulated to provide the optimal combination of chemical resistance, bristle retention, strength, stiffness, processability, clarity, colorability, and feel for toothbrushes. Under existing United States Food and Drug Administration(FDA) regulations, EASTAR BR003 copolyester may lawfully be used to make food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240. Migration tests on BR003 samples meet the compliance requirements of 21 CFR 177.1240(e)(1),(2) and (3).
Applications: Toothbrushes
Technical Data Sheet
General: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given. Information provided by Eastman Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Haze
- Transmission, Visible
- Processing Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|