Eastman EASTAR Copolyester K3000 PETG Copolyester
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Product Description: EASTAR K3000 Copolyester is a cost effective, high-performance, water-clear material that provides the necessary performance for the appliance standards. Other desirable characteristics are good chemical resistance, stiffness, and low shrinkage. In addition, it is "molder friendly" and colors and tints easily.
Applications: Refrigerator interior parts
Technical Data Sheet
Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform to the values give Information provided by Eastman Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Haze
- Transmission, Visible
- Processing Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|