Eastman TENITE Acetate 105E1R26033 Clear, Trsp Cellulose Acetate
Subcategory: Cellulosic; Thermoplastic
Key Words: CA
Material Notes: Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570. Product Description: TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of TENITE cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. TENITE cellulosic plastics are available in natural, clear, amber, and black. Color concentrates are available in let-down ratios from 10:1 to 40:1. TENITE Cellulose Acetate 105-33 is heat stabilized and has a plasticizer level of 33%.
Applications: Housewares; Ophthalmic; Tool handles; Toys/Sporting goods
Technical Data Sheet
Characteristics: Formula 105 - heat stabilized.
Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values give Information provided by Eastman Chemical.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Refractive Index
- Haze
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|