|   Eastman TENITE Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate  Subcategory: Cellulosic; Thermoplastic Key Words: CAP Material Notes: Plasticizer 12%.  Weight loss on heating = 0.5% per ASTM D 707.  Soluble matter loss = 0.1% per ASTM D 570.
 Product Description:  TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of TENITE cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. TENITE cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. TENITE Cellulose Acetate Propionate 350-14 has a plasticizer level of 14%.  It meets FDA requirements when supplied in FDA numbers.
 Applications:  Medical
 
 Technical Data Sheet
 
 Characteristics:  Formula 350 - base
 
 Comments:  Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.
 Information provided by Eastman Chemical. 
| | 
    | Available Properties |  
    | DensityWater AbsorptionLinear Mold ShrinkageHardness, Rockwell RTensile Strength, UltimateTensile Strength, YieldElongation at BreakFlexural ModulusFlexural Yield StrengthIzod Impact, NotchedIzod Impact, Notched, Low TempElectrical ResistivityDielectric ConstantDielectric StrengthDissipation FactorCTE, linear 20°CSpecific Heat CapacityThermal ConductivityDeflection Temperature at 0.46 MPa (66 psi)Deflection Temperature at 1.8 MPa (264 psi)Vicat Softening PointRefractive IndexHazeTransmission, Visible
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |