E-A-R Specialty Composites VersaDampâ„¢ V-2325 TPE

 

Subcategory: Elastomer, TPE; Thermoplastic

Material Notes:
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded into a wide variety of standard or custom isolators, including grommets, equipment mounts, bumpers, and gaskets. They feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection for sensitive mechanisms within minimum sway parameters, and quick return to equilibrium after vibrations or shocks.

Information provided by Aearo E-A-R Specialty Composites.

Available Properties
  • Hardness, Shore A
  • Tensile Strength @ Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Yield Strength
  • Compressive Modulus
  • Resilience
  • Tear Strength
  • Compression Set
  • Maximum Service Temperature, Air
  • Brittleness Temperature
  • Flammability, UL94
  • MVSS 302 Flammability
  • Relative Peak Transmissibility
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。