E-A-R Specialty Composites Isoloss® HDF Polyurethane Elastomer
Subcategory: Elastomer, TS; Polyurethane, TS; Thermoset
Material Notes: Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection for sensitive mechanisms within minimum sway parameters, and quick return to equilibrium after vibrations or shocks. Information provided by Aearo E-A-R Specialty Composites.
| Available Properties |
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Resilience
- Maximum Service Temperature, Air
- Brittleness Temperature
- Flammability, UL94
- Abrasion Resistance
- Compression Set Resistance
- Damping T max
- Heat Aging; 100°C
- Tear Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|