Hifor Clear Polyethylene SC74560-F
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Good toughness, with excellent gloss and clarity
Material Notes: Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produced using this resin exhibit good toughness, with excellent gloss and clarity for a product of this density. SC74560-F is well suited for packaging frozen goods, fruits and vegetables and baked goods List of Applications: - Bakery film
- Frozen food packaging
- Produce bags
Information supplied by the manufacturer. Information from manufacturer data sheet.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Heat Seal Strength Initiation Temperarture
- Haze
- Gloss
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|