Hifor Xtreme Polyethylene SC74845-F

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer

Key Words: Low seal initiation temperature combined with high stiffness

Material Notes:
Hifor Xtreme SC74845-F is a high strength polyethylene designed for blown and cast film extrusion that contains medium slip and high antiblock additives. Films produced using this resin exhibit a unique low seal initiation temperature combined with high stiffness. Other features of this resin include good clarity and good machine direction tear resistance.

List of Applications:

  • Blown film
  • Cast film
  • Food packaging

Information supplied by the manufacturer.

Information from manufacturer data sheet.

Available Properties
  • Density
  • Thickness
  • Melt Flow
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop
  • Heat Seal Strength Initiation Temperarture
  • Haze
  • Gloss
  • Process
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。