Mxsten CV Plastomer CV77518-F
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Very low seal initiation temperature with a broad hot tack window
Material Notes: Mxsten CV plastomer CV77518-F resin is a polyethylene plastomer designed for blown and cast film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a very low seal initiation temperature with a broad hot tack window. Other features of this resin include higher stiffness, high melting point, and ease of processing for narrow die gaps. List of Applications: - Blown Film
- Cast film
- Packaging
Information supplied by the manufacturer. Information from manufacturer data sheet.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Heat Seal Strength Initiation Temperarture
- Haze
- Gloss
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|