Eastman Chemical Polyethylene 1810F
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: High impact strength, high tear strength and very good optical properties
Material Notes: Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good optical properties, such as packaging for frozen food. List of Applications: - Food packaging
- Food-contact applications
low density polyethylene 1810F may lawfully be used in food-contact applications under FDA regulations at 21 CFR 177.1520(c)(2.2). Information supplied by the manufacturer. Information from manufacturer data sheet.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|