Eastman Chemical Polyethylene 1924P
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Low neck-in, ease of processing, good chill-roll release, low coefficient of friction and good heat sealability
Material Notes: Low-density polyethylene 1924P is a resin in the boardstock coating industry for use in breadboard, cupstock, and liquid packaging board. This material has an excellent combination of low neck-in, ease of processing, good chill-roll release, low coefficient of friction (for ease of indexing carton blanks) and good heat sealability. It is characterized by high-speed processability, excellent drawdown and reliable lot-to-lot consistency. List of Applications: - Food-contact applications
- Photographic paper
Information supplied by the manufacturer. Information from manufacturer data sheet.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|