Eastman Chemical Polyethylene 800E
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Good stress-crack resistance
Material Notes: Polyethylene 800E is used in general-purpose extrusion applications that also require good stress resistance. This formula complies with FDA regulations at 21 CFR177.1520 (c)(2.2) for use in articles for packing and holding food during cooking. Users must make their own determination that their use of this product is safe, legal, and technically suitable for their intended applications. Unless otherwise noted, all tests are run at 23°C and 50% RH. Information from manufacturer data sheet.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|