Eastman Chemical Polyethylene 808A
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: General-purpose formulation
Material Notes: Low density polyethylene 808A is a general-purpose formulation used for injection molding and general-purpose extrusion. Unless otherwise noted, all tests are run at 23°C and 50% RH. Information from manufacturer data sheet.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|