Eastman Chemical Polyethylene 808P
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: General-purpose formulation
Material Notes: Low density polyethylene 808P is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seals at high packaging or sealing rates. Unless otherwise noted, all tests are run at 23°C and 50% RH. Information from manufacturer data sheet.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|