Eastman Chemical Polyethylene 811E
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Flexible, easy molding formula
Material Notes: Extrusion grade; no additives. 811E as supplied by Eastman Chemical may lawfully be used in food contact (noncooking) subject to FDA 21 CFR 177.1520(c)(2.1). Information from manufacturer data sheet.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|