Eastman Chemical Polyethylene D4052-F
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Impact strength, outstanding clarity, and good tear resistance
Material Notes: D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance. This product is suggested for packaging frozen foods and for similar applications requiring toughness and clarity. Information from manufacturer data sheet.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|