Eastman Chemical Polyethylene E6838-850P
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Good adhesion to paper, good moisture barrier, heat-sealable at low temperatures
Material Notes: E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seals at high packaging or sealing rates. It also demonstrates a good adhesion to paper, provides a good moisture barrier and is heat-sealable at low temperatures. List of Applications: - Coatings for paper/paperboard
- Food-contact applications
Information supplied by the manufacturer. Information from manufacturer data sheet.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|