Eastman Chemical Polyethylene E6838-862A
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: Injection molding applications, such as closures
Material Notes: E6838-862A is a low density formulation suggested for injection molding applications, such as closures Information supplied by the manufacturer. Information from manufacturer data sheet.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|