Eastman Chemical Polyethylene E6838-923F

 

Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer

Key Words: Medium antiblock, good heat seal, low slip

Material Notes:
E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarity is important. Common applications include bread bags, fresh produce bags, and convertor film requiring printability. As supplied by Eastman Chemical, Polyethylene E6838-923F may lawfully be used in food-contact applications under the FDA regulations at 21 CFR177.1520 (c)(2.2). An additive in this formulation limits the use of E6838-923F to nonalcoholic foods, and the average thickness of such polymers in the form in which they contact food shall not exceed 0.0050 inch. Users must make their own determination that their use of this product is safe, legal, and technically suitable for their intended applications.

CO2 permeability 200 cc-mm/m²-24h-atm (506 cc-mil/100in²-24h-atm). Unless otherwise noted, all tests are run at 23°C and 50% RH. Extrusion conditions used to produce blown film: 1.9:1 blow-up ratio.

Information from manufacturer data sheet.

Available Properties
  • Density
  • Moisture Vapor Transmission
  • Thickness
  • Melt Flow
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Coefficient of Friction
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop
  • Vicat Softening Point
  • Haze
  • Gloss
  • Transmission, Visible
  • Process
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。